| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ±0.02 g/cm³; DIN 53479 |
| Water Absorption | 2.8 % | 2.8 % | 23C/50RH; ISO 62 |
| Water Absorption at Saturation | 8.5 % | 8.5 % | ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 80.0 MPa @Temperature 23.0 °C |
11600 psi @Temperature 73.4 °F |
dry as moulded; ISO 527-2/50 |
| Elongation at Yield | 4.5 % @Temperature 23.0 °C |
4.5 % @Temperature 73.4 °F |
dry as moulded; ISO 527-2/50 |
| Tensile Modulus | 3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
dry as moulded; ISO 527-2/1 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
| NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 261 °C | 502 °F | ISO 3146 |
| Maximum Service Temperature, Air | 90.0 °C | 194 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 200 °C | 392 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-2 @Thickness 0.800 mm |
V-2 @Thickness 0.0315 in |
UL 94 |
| Glow Wire Test | 650 °C @Thickness 0.800 mm |
1200 °F @Thickness 0.0315 in |
uncolored material; Ignition Temperature; IEC 60695-2-13 |
| 750 °C @Thickness 0.800 mm |
1380 °F @Thickness 0.0315 in |
Flammability Index; uncolored material; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.6 @Frequency 1.00e+6 Hz |
3.6 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 120 kV/mm | 3050 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.026 @Frequency 1.00e+6 Hz |
0.026 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 270 - 290 °C | 518 - 554 °F | |
| Mold Temperature | 40.0 - 80.0 °C | 104 - 176 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | Desiccant Dryer |
| Back Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Processing Method | Extrusion | |
| Injection Molding | ||
| Regional Availability | Asia Pacific | |
| Europe | ||
| North America | ||
| RoHS Compliance | RoHS Compliant | |
| UL File Number | E76261 | Global |