| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE)
OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 52G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN52G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provide..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 52GM50EF WT001 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN52GM50EF WT001 is a glass and mineral reinforced high performance polyamide resin developed for LED reflector applications. It is also a PPA resin.Information provided by DuPont Performan..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
|
|||
| Dry Time |
4.00
-
8.00
hour <br>@Temperature 120 °C
|
4.00
-
8.00
hour <br>@Temperature 248 °F
|
|
|
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||
| Dry Time |
4.00
-
8.00
hour <br>@Temperature 120 °C
|
4.00
-
8.00
hour <br>@Temperature 248 °F
|
|
|
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Dry Time |
4.00
-
8.00
hour <br>@Temperature 120 °C
|
4.00
-
8.00
hour <br>@Temperature 248 °F
|
|
|
Lanxess Pocan® KU 2-7241 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, flame retardant, improved impact strengthInformation provided by LANXESS.
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® 2533 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® 2533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® 2533 SD 02 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 2533 SD 02 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SD grade is heat and UV stabilized and contains mold release additive.Infor..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® 3533 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 3533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® MV 1041 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 1041 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on ..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | Handling |
|
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | Handling |
|
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled
These epoxy and urethane based coatings are used for producing corrosion and wear resistant barriers to 500°F. Typical applications include tanks, piplines, boilers, precipitators, scrubbers, bag h..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | Touch |
|
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | Recoat |
|
Aremco Corr-Paint™ CP2060 High Temperature Protective Coating Novolac-Epoxy, Silicon Carbide Filled
This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | Recoat |
|
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled
Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C).
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 54G35EF NC010 Polyphthalamide (PPA)
Zytel® HTN54G35EF NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin, developed for electrical and electronics applications. It is also a PPA r..
|
|||
| Dry Time | 4.00 - 8.00 hour | 4.00 - 8.00 hour | |
|
Arkema Group Pebax® Rnew 35R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 35R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFR52G30NHF BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin with improved flow. It is also a PPA resin and it uses a non-halogenated flame ret..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont ..
|
|||
| Dry Time |
4.00
-
8.00
hour <br>@Temperature 120 °C
|
4.00
-
8.00
hour <br>@Temperature 248 °F
|
|
|
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin..
|
|||
| Dry Time | 6.00 - 8.00 hour | 6.00 - 8.00 hour | DAM |
|
DuPont Performance Polymers Zytel® HTN FE8200 BK431 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTNFE8200 BK431 is an unreinforced, toughened, heat stabilized, lubricated high performance polyamide resin for injection molding. It is also a PPA resin.Information provided by DuPont Perfo..
|
|||