Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending, tensial strength, toughness. Does not absorb water, that means that identical properties are maintained also in wet environment. Melt is characterised by very good rheology, which enables manufacturing of extremely multiple products with complicated downflow-path. Anisotropy of shrinkage is much better in comparison with PA, what influences the manufacturing of round, cylindric or other hole products. Application in the automotive, electrical and engineering industry - connectors of cable harnesses, car-door locks, connection links, grips etc. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
Viscosity Measurement 97
97
Linear Mold Shrinkage 0.0061 cm/cm
0.0061 in/in
Linear Mold Shrinkage, Transverse 0.0067 cm/cm
0.0067 in/in
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 250 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 11.5 GPa
1670 ksi
Flexural Strength 220 MPa
31900 psi
Flexural Modulus 8.50 GPa
1230 ksi
Charpy Impact Unnotched 6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
6.50 J/cm²

@Temperature -20.0 °C
30.9 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 224 °C
435 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Vicat Softening Point 215 °C
419 °F
Flammability Test 1.0
1.0
Glow Wire Test 750 °C
1380 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 33.0 kV/mm
838 kV/in
Comparative Tracking Index 500 V
500 V
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour
Moisture Content 0.050 %
0.050 %
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi
Copyright © lookpolymers.com All Rights Reserved