Potters Industries Conduct-O-Fil® SN08P40 Silver-coated Sub-10 micron Particles

Category Ceramic , Glass , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Potters Industries
Trade Name Conduct-O-Fil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Potters Industries Conduct-O-Fil® SN08P40 Silver-coated Sub-10 micron Particles.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Conduct-O-Fil® conductive particles are engineered to meet a broad range of conductive and electro magnetic interference requirements. A variety of particle shapes offers the formulator additional flexibility in achieving optimum particle performance.Information provided by Potters Industries.
Physical Properties Metric English Comments
Particle Size 8.0 µm
8.0 µm
Average Diameter
Component Elements Properties Metric English Comments
Silver, Ag 40 %
40 %
by weight
Descriptive Properties Value Comments
Core Material Nickel