Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucite International Diakon® TD542 Toughened Acrylic Compound

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Lucite International
Trade Name Diakon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Diakon® TD542 Toughened Acrylic Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by injection molding or extrusion.Information provided by Lucite International
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 0.90 g/10 min
0.90 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell M 25
25
ISO 2039-2
Tensile Strength 45.0 MPa
6530 psi
ISO 527
Elongation at Break 35 %
35 %
ISO 527
Flexural Modulus 1.70 GPa
247 ksi
ISO 178
Izod Impact, Notched (ISO) 5.20 kJ/m²
2.47 ft-lb/in²
ISO 180/1A
Charpy Impact, Notched 0.480 J/cm²
2.28 ft-lb/in²
ISO 179/1eA
5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear 123 µm/m-°C
68.3 µin/in-°F
ASTM E831
Vicat Softening Point 94.0 °C
201 °F
ISO 306B
108 °C
226 °F
ISO 306A
Heat Distortion Temperature 91.0 °C
196 °F
ISO 75A
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
IEC 695-2-1
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ISO 489
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003
Users viewing this material also viewed the following: