| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 93.9 °C | 201 °F | ASTM D-1525 |
| Plaskolite Optix® CP - 51 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
| Vicat Softening Point | 93.9 °C | 201 °F | ASTM D-1525 |
| Plaskolite West Optix® CA - 51 FDA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
| Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
ISO 306/A |
| Polimeri Europa Riblene® FM 34 Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 is characterized by a good balance between processabilit.. |
|||
| Vicat Softening Point | 94.0 °C @Load 1.00 kg |
201 °F @Load 2.20 lb |
ISO 306/A |
| Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Eastman 1830A Polyethylene
(discontinued **) Polyethylene 1830A is a low density formulation. It is suggested for injection molding applications requiring good stiffness or gloss properties . It us used in applications such as closures.Polyet.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Vicat Softening Point | 94.0 °C @Load 5.00 kg |
201 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| LG Chemical SH610A ABS, High Impact Feature: Extrusion Molding, General Purpose, High ImpactApplication: Bag, Automobile InteriorCAS No. 9003-56-9Information provided by LG Chemical |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ISO 306B |
| Lucite International Diakon® TD542 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics NORYL RN0401 PPE+PS (Asia Pacific) RN0401 is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 20% PCR styrenic series resin content. Available in black only. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
| Samsung Cheil Industries Starex® VS-0800 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | (50 °C/h / 50N) - B/50; ISO 306 |
| Styrolution Terluran® HI-10 ABS Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | B/50; ISO R306 |
| Samsung Cheil Industries Starex® GC-0710 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | 50B; ISO 306 |
| Sax Polymers SAXATEC 6120 AES SAXATEC 6120 is a easy lowing, weatherable AES injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym.. |
|||
| Vicat Softening Point | 94.0 °C @Load 1.02 kg |
201 °F @Load 2.25 lb |
50°C per hour; ASTM D1525 |
| Total PS CPDS 855S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 855S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | A50; DIN 53460 |
| Lubrizol ESTANE® 58156 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp Applications:OphthalmicsOptical safety framesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, cla.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | 50°C/h 50N; ISO 306 |
| Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content |
|||
| Vicat Softening Point | 93.9 °C | 201 °F | 0.125 inch, 1 Kg; ASTM D1525 |
| Diamond Polymers ASA S319 Description: ASA Weatherable Polymer, Injection Molding Grade, High ModulusInformation provided by Diamond Polymers, Inc. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | |
| BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
| Vicat Softening Point | 93.9 °C | 201 °F | ASTM D1525 |
| Americas Styrenics MC3700 High Heat Crystal Polystyrene Product CharacteristicsEasy filling of thin-walled partsExceptional mold releaseImproved cycle times in hard to fill partsFood Contact CompliantUL Classification 94HBUSP Class VITypical Applications.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | 49 N; ISO 306 |
| A.D. Compound Adene NTFA Homopolymer 20% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | ASTM D1525 |
| Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
| Vicat Softening Point | 94.0 °C | 201 °F | 49 N; ISO 306 |
| A.D. Compound Adene NCHA Homopolymer 25% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||