| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Glow Wire Test |
650
°C <br>@Thickness 3.00 mm
|
1200
°F <br>@Thickness 0.118 in
|
STN EN 60695-2-12 |
|
Plastcom PLASTAMID® 6 GF 30 031 TS PA6 reinforced with glass fiber, heat stabilized
PA 6 for injection molding, reinforced with 30% glass fiber, heat stabilized, better surface appearance of injection moldings. Decrease in tensile strength by 50 % after 5000 hours at 170°C. Used f..
|
|||
| Glow Wire Test | 650 °C | 1200 °F | |
|
Plastcom SLOVAMID 6 GF 60 000/1M PA6 reinforced with 60% glass fibre
Features: PA 6 for injection moulding, chemically strengthened with 60% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.00 mm
|
1200
°F <br>@Thickness 0.0394 in
|
Flammability Index; IEC 60695-2-12 |
|
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
|
|||
| Glow Wire Test | 650 °C | 1200 °F | STN IEC 60695-2-10 |
|
Plastcom SLOVAMID 66 GF 25 Polyamide 66, 25% Glass Fiber
FeaturesChemically reinforced with 25% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Glow Wire Test | 650 °C | 1200 °F | |
|
Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delive..
|
|||
| Glow Wire Test | 650 °C | 1200 °F | |
|
Plastcom SLOVAMID 66 GF 45 PA66, 45% glass fibre
FeaturesChemically reinforced with 45% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.60 mm
|
1200
°F <br>@Thickness 0.0630 in
|
IEC 60695-2-1 |
|
Polimeri Europa Edistir N 1840 Polystyrene
General purpose polystyrene combining easy flow and medium heat. Edistir N 1840 is suggested in extrusion for glossy capping of HIPS sheets and for blending with HIPS or clear SBS for stiffer therm..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.00 mm
|
1200
°F <br>@Thickness 0.0394 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East)
CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.00 mm
|
1200
°F <br>@Thickness 0.0394 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Cycolac® GPM5500F ABS (Europe-Africa-Middle East)
CYCOLAC GPM5500F is a multi purpose injection moulding grade, providing a favourable balance of engineering properties and is FDA and European Directive 2002/72/EC
(FCEU) compliant for food contac..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 695-2-1 |
|
Polykemi AB POLYabs N30 ABS
Information provided by Polykemi AB
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
IEC 695-2-1 |
|
Polykemi AB POLYfill PPC GF2007 PD1 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 1.00 mm
|
1200
°F <br>@Thickness 0.0394 in
|
Glow Wire Flammability Index; IEC 60695-2-12 |
|
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 695-2-1 |
|
Polykemi AB SCANAMID 66 A12^ F20 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 695-2-1 |
|
Polykemi AB SCANMID 6 B/C12^ F30 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 695-2-1 |
|
Polykemi AB SCANMID 6 B12^ QF2515 Nylon 6, Glass Fiber and Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Glow Wire Test |
650
°C <br>@Diameter 2.00 mm
|
1200
°F <br>@Diameter 0.0787 in
|
GWFI; IEC 60695-2-12 |
|
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
|
Lucite International Diakon® CMG334V Acrylic Polymer
Information provided by Lucite International
|
|||
| Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
|
Lucite International Diakon® LG703 Acrylic Bead Polymer, High Transparency
PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 3.20 mm
|
1200
°F <br>@Thickness 0.126 in
|
IEC 60695-2-12 |
|
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East)
VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks.
|
|||
| Glow Wire Test | 650 °C | 1200 °F | IE/CEN 60695-2-12 |
|
Sax Polymers SAXLAC 120T Acrylonitrile Butadiene Styrene
Saxalac 120T is an antistatic, easy flowing ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical property data tested ..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
I.E.C. 695-2-1 |
|
Cossa Polimeri ESTADIENE 0425 GFS Acrylonitrile Butadiene Styrene, 13% Glass Filled
ABS with 13% short glass fiberExcellent mechanical and thermal propertiesInformation provided by Cossa Polimeri S.r.l.
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
I.E.C. 695-2-1 |
|
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
I.E.C. 695-2-1 |
|
Cossa Polimeri ESTADIENE 1640 AS Acrylonitrile Butadiene Styrene
General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 60695-2-12 |
|
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded
Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
plaque; IEC 60695 |
|
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
plaque; IEC 60695 |
|
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
plaque; IEC 60695 |
|
Eurotec® Tecomid® NB40 GR25 NL PA 6 25% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Glow Wire Test |
650
°C <br>@Thickness 2.00 mm
|
1200
°F <br>@Thickness 0.0787 in
|
IEC 695-2-1 |
|
Polykemi AB POLYfill PPC 15000 Polypropylene Copolymer
Information provided by Polykemi AB
|
|||
| Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
|
Lucite International Diakon® Frost 902 80 Acrylic Polymer
Information provided by Lucite International
|
|||