Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 0.90 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Clearflex® FG B3 Very Low Density Polyethylene
Clearflex FG B3 is a linear low density polyethylene, with antioxidants, slip and antiblocking agents, suitable for blown film technology. The product is characterized by a very low density and a h..
Melt Flow 0.90 g/10 min
0.90 g/10 min
Condition E; ASTM D 1238
Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Slip, Very High Antiblock Version of 7109T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
Chevron Phillips 6109FK Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, butene copolymer, medium antiblock, medium slip, process aid version of 6109, blown film resinCharacteristics: good stiffness at thin gauges, good drawdo..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® FORMAX® L71709H Film (Hexene Grade) LLDPE  (discontinued **)
High Strength Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L7 is a high strength linear low density hexene copolymer polyethylene made using a gas-phase process. Film mechan..
Melt Flow 0.90 g/10 min
0.90 g/10 min
Exxon Method
ExxonMobil Escorene® LD-315 EVA Packaging Film Resin for Frozen Food  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 5.0% vinyl acetate copolymer clarity film resin. This resin's low melt index and its comonomer contact combine to provide film of special toughne..
Melt Flow 0.90 g/10 min

@Load 2.16 kg
0.90 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Reclair F19010 Polyethylene
Blow film Linear Low Density Polyethylene grade. Reclair F19010 is butene comonomer based, with optimum levels of antioxidants, antiblocking agents, slip additives, and polymer processing aids. Th..
Melt Flow 0.90 g/10 min

@Load 2.16 kg
0.90 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Reclair O21010 Polyethylene
Octene comonomer based Linear Low Density Polyethylene. Blow film grade. Contains an optimum level of antioxidants and polymer processing aids. Designed for lamination film applications. Character..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
LyondellBasell Adflexâ„¢ KS-021P TPO Resin
Primary Processing Method: Blown Film/Impact ModificationKey Features: excellent low temperature impact resistance, excellent chemical and environmental stress-cracking resistance, FDA acceptable, n..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) LL0209 KJ Linear Low Density Polyethylene
LL 0209 is a LLDPE copolymer with butene as comonomer which contains anti-oxidant, Slip and antiblock additives. It gives film of high slip which is easily separable. It is recommended for general ..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene
LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co.
Melt Flow 0.90 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.90 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Samsung Cheil Industries Starex® HR-0370F ABS, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BB108E Polypropylene compound for Steel Pipe Coating
BB108E is a high molecular weight, low melt flow rate polypropylene block copolymer. Applications: BB108E is recommended for steel pipe coating.Information provided by Borealis AG
Melt Flow 0.90 g/10 min
0.90 g/10 min
LE 4421; ASTM D1238
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination o..
Melt Flow 0.90 g/10 min
0.90 g/10 min
LE 4423; ASTM D1238
Borealis Visico™ LE4423/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Visico LE4423/LE4437 is a mature, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base materia..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product
DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman.
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product
DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman.
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Total Lumicene® mPE M 3410 EP HDPE Film
Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238E
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238E
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
ExxonMobil NTX™ NTX 101 Super Strength Film Resin
NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly..
Melt Flow 0.90 g/10 min
0.90 g/10 min
ASTM D1238
ExxonMobil NTX™ NTX 141 Super Strength Film Resin
NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impac..
Melt Flow 0.90 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.90 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers SAN 250 Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 235 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 455 °F
after drying; ISO 1133
Arkema Group Orgalloy® LE 60 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
M. Holland Company LL106 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH..
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
E-Polymers EFLEX® S5060 Extrusion
S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas..
Melt Flow 0.90 g/10 min
0.90 g/10 min
Condition L; ASTM D1238
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade
80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar..
Melt Flow 0.90 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.90 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® ME3444 Blue Medium Density Polyethylene for Drinking Water Pipes
Borstar 3444 is a blue, bimodal, medium density polyethylene classified as a MRS 8.0 material (PE80) produced with the advanced Borstar technology. A combination of pigments and stabilizers is incl..
Copyright © lookpolymers.com All Rights Reserved