| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled |
| Manufacturer | LTL Color Compounds |
| Trade Name | ColorFast® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.19 g/cc | 1.19 g/cc | ASTM D792 |
| Water Absorption | 1.5 % | 1.5 % | @ 24 Hours; ASTM D570 |
| Linear Mold Shrinkage | 0.0030 - 0.010 cm/cm | 0.0030 - 0.010 in/in | 0.125; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 115 | 115 | ASTM D785 |
| Tensile Strength, Yield | 75.8 MPa | 11000 psi | 2.0 in/min; ASTM D638 |
| Elongation at Break | 15 % | 15 % | 2.0 in/min; ASTM D638 |
| Elongation at Yield | 7.0 % | 7.0 % | 2.0 in/min; ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | 2.0 in/min; ASTM D790 |
| Flexural Modulus | 4.14 GPa | 600 ksi | 2.0 in/min; ASTM D790 |
| Izod Impact, Notched | 1.33 J/cm @Temperature 22.8 °C |
2.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 221 °C | 430 °F | Unannealed (0.250"); ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
| Middle Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
| Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
| Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
| Melt Temperature | 279 - 304 °C | 535 - 580 °F | |
| Mold Temperature | 37.8 - 93.3 °C | 100 - 200 °F | |
| Drying Temperature | 82.2 °C | 180 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | nominal; maximum drying time of 8 hours |
| Back Pressure | 0.345 - 0.689 MPa | 50.0 - 100 psi | |
| Shot Size | 30 - 60 % | 30 - 60 % | |
| Vent Depth | 0.00381 - 0.00762 cm | 0.00150 - 0.00300 in | |
| Screw Speed | 60 - 120 rpm | 60 - 120 rpm |