| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| NYCOA 2062 Copolymer Nylon 6/66 FDA approved extrusion grade for film.Information provided by NYCOA, Inc. |
|||
| Izod Impact, Notched | 0.400 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.749 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
| PolyOne LubriOne™ NN-000/10T-2S Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| NCMT NanoPAC™ S301 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi.. |
|||
| Izod Impact, Notched | 0.400 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.749 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256 |
| PolyOne Geon™ L4605 Red 7640 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | 23° C; ASTM D256 |
| Flint Hills P5L2Z-038 Random Copolymer Polypropylene Random copolymer, USP Class VI certified, and FDA compliant.Features: Hydrotalcite.Applications: Injection molding: extrusion blow molding and hot fill applications.Former Huntsman polypropylene pro.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
| Izod Impact, Notched | 0.400 J/cm @Temperature 23.0 °C |
0.749 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
| Izod Impact, Notched | 0.400 J/cm @Thickness 3.17 mm |
0.750 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES HiFill® PA4/6 0206 Availability: North AmericaForms: PelletsFeatures: High Specific Gravity and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3707 is a 20% CAC03 filled homopolymer polypropylene product.Information provided by A. Schulman. |
|||
| Izod Impact, Notched | 0.400 J/cm @Temperature 23.0 °C |
0.749 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
| Polyram PlusTek RA325J5 Nylon 6.6, 25% Glass beads and Glass Fiber, Flame Retardant 25% glass beads and glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Izod Impact, Notched | 0.400 J/cm @Thickness 3.17 mm |
0.749 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Washington Penn PPH3TF4-BLK Polypropylene, 40% Talc Filled Homopolymer. Meets GMP.PP.030 spec.Applications: Fan shrouds, heater housings, various under hood uses.Data provided by Washington Penn Plastic Co., Inc. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ISO 180 |
| Wellman Wellamid® GS40-60 42L-N 40% Glass Sphere Filled Nylon 6, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.750 ft-lb/in | |
| Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound TRA-BOND 2112 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.750 ft-lb/in | |
| Tra-Con Tra-Bond 2104 Rigid Epoxy Staking Compound TRA-BOND 2104 is a thixotropic epoxy system recommended for critical electronic, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
| Izod Impact, Notched | 0.400 J/cm @Temperature -40.0 °C |
0.749 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| Eastman Neostar FN007 Elastomer Neostar FN007 elastomer is the third in Eastman’s series of tough, clear, durable copolyester ethers. Though originally designed for use in the profile and automotive markets, this innovative copol.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | |
| Abatron AboCast 8-3/Abocure 8-3 Epoxy 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.750 ft-lb/in | ASTM D256 |
| Aclo Accutech Polypropylene Homopolymer HP0339G10M20CL Glass/Mineral Reinforced Coupled |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Adell BL-38 Nylon 6, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Adell EZ-14 Homopolymer Polypropylene, 20% Calcium Carbonate Filled Data provided by Adell Plastics, Inc. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.749 ft-lb/in | ASTM D256 |
| Carmel Olefins CAPILENE® QW 73 AV Propylene Random Copolymer Description: CAPILENE® QW 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QW 73 AV is clarified with antista.. |
|||
| Izod Impact, Notched | 0.400 J/cm @Temperature -40.0 °C |
0.749 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
| BASF Ultramid® B3GM35 Q643 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid B3GM35 Q643 is a 40% combined glass-fiber and mineral reinforced injection molding PA6 grade. |
|||
| Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | IS 13411-1992 |
| Amity Thermosets ATS 135 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics: Self lubricating Good mechanical strength Low co-efficient of friction Good thermal conductivity Heat stable (200°C) Good mouldability Not suitable for electrical application Color.. |
|||
| Izod Impact, Notched | 0.400 - 0.500 J/cm | 0.749 - 0.937 ft-lb/in | IS 13411-1992 |
| Amity Thermosets ATO 159 Phenolic Molding Glass/ inorganic Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.750 ft-lb/in | |
| Atom Adhesives AA-BOND 2112 Epoxy Adhesive AA-BOND 2112 is a thixotropic epoxy system recommended for critical electronics, aerospace and industrial bonding, laminating and reinforcing applications requiring an adhesive with high-fill, non-s.. |
|||
| Izod Impact, Notched | 0.400 J/cm | 0.750 ft-lb/in | At 73°F; ASTM D256 |
| Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
| Izod Impact, Notched | 0.400 - 0.5339 J/cm @Temperature -40.0 - -20.0 °C |
0.749 - 1.000 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.445 J/cm Grade Count:2 |
| Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
| Izod Impact, Notched | 0.400 - 1.30 J/cm @Temperature -28.9 - -20.0 °C |
0.749 - 2.44 ft-lb/in @Temperature -20.0 - -4.00 °F |
Average value: 0.854 J/cm Grade Count:5 |
| Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||