| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
|
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced
Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Linear Mold Shrinkage |
0.0070
-
0.0090
cm/cm <br>@Temperature 121 °C,<br> Time 3600 sec
|
0.0070
-
0.0090
in/in <br>@Temperature 250 °F,<br> Time 1.00 hour
|
48 hours after molding; ISO 294-3/4 |
|
Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled
AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g..
|
|||
| Linear Mold Shrinkage |
0.0070
-
0.012
cm/cm <br>@Thickness 3.00 mm
|
0.0070
-
0.012
in/in <br>@Thickness 0.118 in
|
ASTM D955 |
|
Samyang Triloy® 410 PC/PET alloy
(discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
|
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled
Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested ..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.014 cm/cm | 0.0070 - 0.014 in/in | FRISETTA Test Method |
|
Nilit FRIANYL B63 GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.0080 cm/cm | 0.0070 - 0.0080 in/in | ASTM D955 |
|
Covestro Apec® DP9-9343 High-Heat Polycarbonate, UV Stabilized
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **)
Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **)
Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i..
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ASTM D955 |
|
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin
G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon.
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D1299 |
|
Loxim 820 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.0090 cm/cm | 0.0070 - 0.0090 in/in | ASTM D1299 |
|
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.010 cm/cm | 0.0070 - 0.010 in/in | ASTM D955 |
|
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Techmer ES Plaslube® PC-50/TF/13/SI/2 BK3585 Polycarbonate |
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
Styron Pulse® 1310 ABS + Polycarbonate
PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
Styron Pulse® 930 ABS + Polycarbonate
PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used i..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Techmer ES Plaslube® PC-50/TF/13/SI/2 WT8966 Polycarbonate |
|||
| Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ISO 2577 |
|
Polyram PlusTek PA351M8 Nylon 6.6 for Injection Molding, 40% Mineral Reinforced
40% Minerals Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
|
|||
| Linear Mold Shrinkage | 0.0070 - 0.011 cm/cm | 0.0070 - 0.011 in/in | ISO 294-4 |
|
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized
Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Lubrizol Estane® R195A Thermoplastic Polyurethane
Type: Estane® R195A is a Shore 95A, polyether type thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: Americas, Europe, Mid..
|
|||
| Linear Mold Shrinkage |
0.0070
cm/cm <br>@Thickness 3.175 mm
|
0.0070
in/in <br>@Thickness 0.1250 in
|
ASTM D955 |
|
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized
Information provided by Asahi Thermofil
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
Asahi Kasei Thermylene® P1-25FM-Y175 25% Glass Fiber/ Mineral Reinforced
Information provided by Asahi Thermofil
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | Compression; ASTM D955 |
|
Chang Chun Plastic Longlite PM T373J Electrical Phenolic Molding Compound
ASTM Grades per ASTM D700 are 2, 3.Information provided by Dowell Trading Company Ltd.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | Dry; ASTM D2863 |
|
Asahi Kasei Leona® 14G15 15% Glass Filled Nylon 66
15% Glass Fiber Reinforced. Enhanced strength and stiffnessApplications:Heater tanks, fuel injectors, ABS sensors, and other under-the-hood automotive parts Information provided by Asahi Kasei
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
|
A. Schulman ComAlloy Comtuf® 631 Nylon 6/6, Glass Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int..
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | |
|
E-Polymers Tekaloy® T80G20 , 20% Glass Fiber Reinforced PBT/ABS Alloy
20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
|
|||
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | Compression; ASTM D955 |
|
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **)