| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced, Flame Retardant |
| Manufacturer | Eurostar Engineering Plastics |
| Trade Name | Starflam |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurostar Starflam PX06091 PA6, Flame Retardant, Injection Molded.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.010 cm/cm <br>@Thickness 4.00 mm |
0.010 in/in <br>@Thickness 0.157 in |
E2P method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 78.0 MPa | 11300 psi | 50 mm/min; ISO 527 |
| Elongation at Break | 5.6 % | 5.6 % | 50 mm/min; ISO 527 |
| Elongation at Yield | 3.7 % | 3.7 % | 50 mm/min; ISO 527 |
| Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 105 MPa | 15200 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 75.0 µm/m-°C <br>@Temperature 23.0 - 60.0 °C |
41.7 µin/in-°F <br>@Temperature 73.4 - 140 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C <br>@Temperature 23.0 - 60.0 °C |
44.4 µin/in-°F <br>@Temperature 73.4 - 140 °F |
ISO 11359-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Bf |
| Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | Flatw 80x10x4, sp=64 mm; ISO 75/Af |
| Flammability, UL94 | V-0 <br>@Thickness 0.750 mm |
V-0 <br>@Thickness 0.0295 in |
|
| Oxygen Index | 32 % | 32 % | ISO 4589 |
| Glow Wire Test | 960 °C <br>@Thickness 0.750 mm |
1760 °F <br>@Thickness 0.0295 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V | 600 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 240 - 250 °C | 464 - 482 °F | |
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
| Drying Temperature | 80.0 °C <br>@Time 14400 sec |
176 °F <br>@Time 4.00 hour |
|
| Moisture Content | 0.20 % | 0.20 % |