Ceradyne CeraTrex™ 146-S5 Silicon Carbide

Category Ceramic , Carbide
Manufacturer Ceradyne Advanced Ceramics
Trade Name CeraTrex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ceradyne CeraTrex™ 146-S5 Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features:corrosion resistancewear resistancehardnessnet shape fabricationApplications:wear componentsInformation provided by Ceradyne Company
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Weibull Modulus 15
15
Mechanical Properties Metric English Comments
Vickers Microhardness 2600
2600
0.3
Modulus of Elasticity 430 GPa
62400 ksi
Flexural Strength 400 MPa

@Temperature 23.0 °C
58000 psi

@Temperature 73.4 °F
Poissons Ratio 0.17
0.17
Fracture Toughness 4.30 MPa-m½
3.91 ksi-in½
Shear Modulus 184 GPa
26700 ksi
calculated
Abrasion 1263
1263
Abrasive Wear Resistance Parameter
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 - 1000 °C
2.50 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+6 ohm-cm
1.00e+6 ohm-cm
Descriptive Properties Value Comments
Purity, % 95
Thermal Shock Parameter 180°C