Polymer Property : CTE, linear, Transverse to Flow = 80.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East)
CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
44.4 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® CY8540 PC+ABS (Europe-Africa-Middle East)
CYCOLOY CY8540 is a PC+ABS blend, especially designed for textile backmolding in automotive interior applications. High flow grade, which allows low temperature processing to maintain fabric integri..
CTE, linear, Transverse to Flow 80.0 - 120 µm/m-°C
44.4 - 66.7 µin/in-°F
Average value: 96.0 µm/m-°C Grade Count:5
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
Covestro Bayblend® R-FR 610 Polycarbonate/ABS Blend &nbsp;(discontinued **)
FR-recycled grades with 25% recycled content.Applications: Housings for office equipment, electrical engineering, computer sectors.Information provided by Bayer.As of 1 September 2015, Bayer Materia..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® KU 1-7635 POS151 000000 PBT + PC, 30% Glass Fiber
PBT+PC, 30% glass fibers, injection molding, low tendency to warp, improved surface finish, UV-stabilized
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duranex® 750LD Polybutylene Terephthalate (PBT), Low warpage, 30% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® FR3010 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® FR3012 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Bayblend® R-FR610 Polycarbonate Recyclate Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame retardantAs of 1 S..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Covestro Makroblend® KU 2-7608 Polycarbonate + PBT, Mineral Filled Impact Grade
ISO 7792-1-PC/PBT,MHPR,-030,MD10(PC+PBT)-blendsimpact modifiedInjection molding grade 10% mineral filledPreprocessingMax. Water content
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® 46HF4130 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, High Flow (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® BGM-40 X PA6-(GF+MD)40
Product description: Grilon BGM-40 X is a heat stabilized PA 6 injection molding grade with a 40 % reinforcement combination (mineral and glass fiber). Grilon BGM-40 X has the following important pr..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TE263F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Impact Modified (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW241F10 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW271F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW275F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified (Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT3Z black 9564 PA*
Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSM-30 PA666-MD30
Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55
Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT) &nbsp;(Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide B28 PA6, Injection Molded
Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBATER BM330 PBT, 30% mineral reinforced, good light reflection
PBT-MD30Information provided by BARLOG plastics GmbH.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)
Ultramid B3WGM24 BK30564 is a 30% glass/mineral filled heat stabilized injection molding PA6 grade for industrial articles having medium to high rigidity and high dimensional stability.
CTE, linear, Transverse to Flow 80.0 µm/m-°C
44.4 µin/in-°F
ISO 11359-1/-2
Covestro Makroblend® DP 6015 Polycarbonate + PBT
Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade. Makroblend DP 6015* provides an outstanding balance of low-temperature impact strength and excellent chemical ..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
<br>@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® GM-20 Acetal Co-polymer (POM), Low warpage, GF 20% reinforced
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend &nbsp;(discontinued **)
Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin..