Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.10 GPa | 450 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 0.1 in/min; ASTM D790 |
Ineos Nova 879 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High heat crystal polystyrene, Color stable, Custom colorsApplications: Injection molding, Designed for applications requiring high strength, high heat resistance, and color stabilityPerformance gra.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
Nilit FRIANYL B63 W-SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
PolyOne Stat-Tech™ AS-15CP/000 ABS - 15% Carbon Powder
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 3.10 GPa @Temperature 90.0 °C |
450 ksi @Temperature 194 °F |
ASTM D790 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 3.10 - 21.0 GPa | 450 - 3050 ksi | Average value: 9.79 GPa Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Modulus | 3.10 - 12.5 GPa | 450 - 1810 ksi | Average value: 7.42 GPa Grade Count:113 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 15 mm/min; ASTM D790 |
LG Chemical 15NFE GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Styrolution PS-148G Polystyrene Description: Polystyrene 148G is a high heat, easy flow general purpose polystyrene with excellent moldability, clarity and fast set-up time. It can be utilized as a coextruded gloss cap over high i.. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Teknor Apex Beetle® 102 Nylon 66, Unreinforced, Nucleated Notes: Nucleated for fast cycling; Improved strength and rigidity; FMVSS Flammability: Passes, FMVSS 302Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very .. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Multibase Multi-Pro® 4007 XGS Polypropylene Mineral, 40% by weight.Features:Gloss, HighScratch ResistantForms:PelletsProcessing Methods:Injection MoldingUses: FurnitureAppliancesInformation provided by Multibase |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ASTM D790 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Flexural Modulus | 3.10 GPa | 450 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermotuf PK003EI2 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* PK003EI2 is a compound based on PA 6 resin containing Impact Modifier, Mineral. Added features include High Impact, Easy Molding.This data was supplied by SABIC-IP for the Europe-Afr.. |