| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass Fiber Filled, Flame Retardant |
| Manufacturer | Eurostar Engineering Plastics |
| Trade Name | Starflam |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Eurostar Starflam BFR430A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0035 - 0.0055 cm/cm | 0.0035 - 0.0055 in/in | on Tensile Bar; E2P method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 85.0 MPa | 12300 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 3.0 % | 3.0 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 6.20 GPa | 899 ksi | 1 mm/min; ISO 527 |
| Flexural Yield Strength | 165 MPa | 23900 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 6.00 GPa | 870 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 4.00 kJ/m² @Temperature -40.0 °C |
1.90 ft-lb/in² @Temperature -40.0 °F |
80x10x4; ISO 180/1A |
| 5.00 kJ/m² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
80x10x4; ISO 180/1A | |
| 6.00 kJ/m² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
80x10x4; ISO 180/1A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 205 °C | 401 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 180 °C | 356 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Ae |
| Vicat Softening Point | 200 °C | 392 °F | B/50; ISO 306 |
| 215 °C | 419 °F | B/120; ISO 306 | |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 300 V | 300 V | IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 1 | 240 - 250 °C | 464 - 482 °F | |
| Zone 2 | 250 - 260 °C | 482 - 500 °F | |
| Zone 3 | 250 - 270 °C | 482 - 518 °F | |
| Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
| Drying Temperature | 80.0 °C @Time 14400 sec |
176 °F @Time 4.00 hour |
|
| Moisture Content | 0.20 % | 0.20 % |