Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 1.45 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
PolyOne OnForce™ LFT NN-40LGF/000 HS Natural Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Polykemi AB SCANAMID 66 A53^ F43 Nylon 66, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
Density 1.45 g/cc
0.0524 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® HTN FG52G35HSL BK011 Polyphthalamide (PPA)  (Unverified Data**)
Zytel®® HTNFG52G35HSL BK011 is a 35% glass reinforced, lubricated, heat stabilized high performance polyamide resin, developed for consideration into applications for the food industry. It is also..
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced
Information provided by Polykemi AB
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Lytex 4149 is a high-performance, 3K tow carbon fiber (PAN) reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical propert..
Density 1.45 g/cc
0.0524 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO R 1184
Fainplast Compounds RH 210/W Rigid PVC, Antishock Extrusion
Various antishock profiles
Density 1.45 g/cc
0.0524 lb/in³
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Density 1.45 g/cc
0.0524 lb/in³
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Density 1.45 g/cc
0.0524 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Lubricomp JL003 PES
LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region.
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear
LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant.
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS - LINEAR
LNP LUBRICOMP* OP005XXC is a compound based on PPS - Linear resin containing 25% PTFE/Silicone. Added features of this material include: Wear Resistant.
Density 1.45 g/cc
0.0524 lb/in³
Dry; ASTM D792
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc.
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific)
LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead.
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183-87
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced
Developmental productAll information provided by Wellman Engineered Resins.
Density 1.45 g/cc
0.0524 lb/in³
dry; ISO 1183
DSM Akulon® K224-G8 PA6-GF40
40% Glass Reinforced
Density 1.45 g/cc
0.0524 lb/in³
DAM; ISO 1183
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance ..
Density 1.45 g/cc
0.0524 lb/in³
IEC 60811
Fainplast Compounds HAX HFX 024-21L Halogen Free PVC
This product is a LSFOH silane grafted compound for cable insulation and sheating, cross-linking by heat and moisture by previous addition of a suitable catalyst masterbatch. It is highly recommende..
Density 1.45 g/cc
0.0524 lb/in³
Aremco Aremco-Seal™ 617 High Temperature Glass Coating
Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC).
Density 1.45 g/cc
0.0524 lb/in³
BASF Paliogen® Red L 3880 HD Color Additive
Description: Perylene reds for shades with high brilliancy and opacitySuitable for: Baking systems, Waterborn systems, Acrylic-isocyanate systems, Acid curing systems, Amine curing systems and Aird..
Density 1.45 - 1.49 g/cc
0.0524 - 0.0538 lb/in³
ISO 1183
Fainplast Compounds Hax™ HF 223F Flame Retardant Polyolefin Cable Compound
Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:High flexibility, good stress crack resistanceInformation provided by Fainplast Compound..
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183/A
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Verton UV007S PPA (Asia Pacific)
LNP VERTON* UV007S is a compound based on Polyphthalamide resin containing Long Glass, Long Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP ..
Density 1.45 g/cc
0.0524 lb/in³
LATI Latilub 66-15ST G/30 PA66, 30% Glass Fiber Reinforced, Silicone/PTFE Filled
Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La..
Density 1.45 g/cc
0.0524 lb/in³
ASTM D-792
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac
FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America...
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES
LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing 10% Glass Fiber.
Copyright © lookpolymers.com All Rights Reserved