| Category | Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.32 g/cc | 0.0477 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 0.30 % <br>@Temperature 23.0 °C |
0.30 % <br>@Temperature 73.4 °F |
Immersion 24h; DAM; ISO 62, Similar to |
| 0.70 % <br>@Temperature 23.0 °C |
0.70 % <br>@Temperature 73.4 °F |
Equilibrium 50%RH; DAM; ISO 62, Similar to | |
| 1.8 % <br>@Temperature 23.0 °C |
1.8 % <br>@Temperature 73.4 °F |
Saturation, immersed; DAM; ISO 62, Similar to | |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm <br>@Thickness 2.00 mm |
0.0030 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.0090 cm/cm <br>@Thickness 2.00 mm |
0.0090 in/in <br>@Thickness 0.0787 in |
DAM; ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 140 MPa <br>@Temperature 23.0 °C |
20300 psi <br>@Temperature 73.4 °F |
50%RH; ISO 527 |
| 168 MPa <br>@Temperature 23.0 °C |
24400 psi <br>@Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 3.2 % <br>@Temperature 23.0 °C |
3.2 % <br>@Temperature 73.4 °F |
DAM; ISO 527 |
| 3.2 % <br>@Temperature 23.0 °C |
3.2 % <br>@Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 7.90 GPa <br>@Temperature 23.0 °C |
1150 ksi <br>@Temperature 73.4 °F |
50%RH; ISO 527 |
| 9.50 GPa <br>@Temperature 23.0 °C |
1380 ksi <br>@Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 7.00 GPa <br>@Temperature 23.0 °C |
1020 ksi <br>@Temperature 73.4 °F |
50%RH; ISO 178 |
| 8.20 GPa <br>@Temperature 23.0 °C |
1190 ksi <br>@Temperature 73.4 °F |
DAM; ISO 178 | |
| Izod Impact, Notched (ISO) | 10.0 kJ/m² <br>@Temperature -30.0 °C |
4.76 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 180/1A |
| 10.0 kJ/m² <br>@Temperature -40.0 °C |
4.76 ft-lb/in² <br>@Temperature -40.0 °F |
50%RH; ISO 180/1A | |
| 11.0 kJ/m² <br>@Temperature -40.0 °C |
5.23 ft-lb/in² <br>@Temperature -40.0 °F |
DAM; ISO 180/1A | |
| 11.0 kJ/m² <br>@Temperature -30.0 °C |
5.23 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 180/1A | |
| 12.0 kJ/m² <br>@Temperature 23.0 °C |
5.71 ft-lb/in² <br>@Temperature 73.4 °F |
50%RH; ISO 180/1A | |
| 13.0 kJ/m² <br>@Temperature 23.0 °C |
6.19 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 45.0 kJ/m² <br>@Temperature -30.0 °C |
21.4 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 180/1U |
| 60.0 kJ/m² <br>@Temperature -30.0 °C |
28.6 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 180/1U | |
| 60.0 kJ/m² <br>@Temperature 23.0 °C |
28.6 ft-lb/in² <br>@Temperature 73.4 °F |
50%RH; ISO 180/1U | |
| 70.0 kJ/m² <br>@Temperature 23.0 °C |
33.3 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 180/1U | |
| Charpy Impact Unnotched | 6.00 J/cm² <br>@Temperature -30.0 °C |
28.6 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eU |
| 6.50 J/cm² <br>@Temperature -30.0 °C |
30.9 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| 8.00 J/cm² <br>@Temperature 23.0 °C |
38.1 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 179/1eU | |
| 9.00 J/cm² <br>@Temperature 23.0 °C |
42.8 ft-lb/in² <br>@Temperature 73.4 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.00 J/cm² <br>@Temperature -30.0 °C |
4.76 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| 1.00 J/cm² <br>@Temperature -40.0 °C |
4.76 ft-lb/in² <br>@Temperature -40.0 °F |
50%RH; ISO 179/1eA | |
| 1.10 J/cm² <br>@Temperature -30.0 °C |
5.23 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 1.20 J/cm² <br>@Temperature 23.0 °C |
5.71 ft-lb/in² <br>@Temperature 73.4 °F |
50%RH; ISO 179/1eA | |
| 1.20 J/cm² <br>@Temperature -40.0 °C |
5.71 ft-lb/in² <br>@Temperature -40.0 °F |
DAM; ISO 179/1eA | |
| 1.30 J/cm² <br>@Temperature 23.0 °C |
6.19 ft-lb/in² <br>@Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 500 µm/m-°C <br>@Temperature -40.0 - 23.0 °C |
278 µin/in-°F <br>@Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 500 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
278 µin/in-°F <br>@Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 500 µm/m-°C <br>@Temperature 55.0 - 160 °C |
278 µin/in-°F <br>@Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| CTE, linear, Transverse to Flow | 83.0 µm/m-°C <br>@Temperature -40.0 - 23.0 °C |
46.1 µin/in-°F <br>@Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
| 113 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
62.8 µin/in-°F <br>@Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 | |
| 158 µm/m-°C <br>@Temperature 55.0 - 160 °C |
87.8 µin/in-°F <br>@Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 | |
| Melting Point | 218 °C | 424 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 216 °C | 421 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
| Glass Transition Temp, Tg | 70.0 °C | 158 °F | 10°C/min; DAM; ISO 11357-1/-2 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
| 280 - 300 °C | 536 - 572 °F | DAM | |
| Mold Temperature | 70.0 - 120 °C | 158 - 248 °F | DAM |
| 100 °C | 212 °F | DAM; optimum | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.15 % | <= 0.15 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Forms | Pellets | DAM |
| Generic | PA612 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA612-GF33< | ISO 11469; DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Food Contact Resins | DAM |
| Glass Reinforced Resins | DAM | |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA612-GF33 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |
| Uses | Food Applications, Non-specific | DAM |