Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ERG Aerospace Reticulated Vitreous Carbon (RVC)

Category Carbon
Manufacturer ERG Aerospace
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ERG Aerospace Reticulated Vitreous Carbon (RVC).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Glass-like Carbon Foam
Physical Properties Metric English Comments
Density 0.0500 g/cc
0.00181 lb/in³
Produced at 3% relative density
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.170 - 1.02 MPa
24.7 - 148 psi
Modulus of Elasticity 0.0310 - 0.0620 GPa
4.50 - 8.99 ksi
Compressive Yield Strength 0.280 - 1.20 MPa
40.6 - 174 psi
Compressive Modulus 0.0310 - 0.0620 GPa
4.50 - 8.99 ksi
Shear Modulus 0.0300 GPa
4.35 ksi
Thermal Properties Metric English Comments
Specific Heat Capacity 1.26 J/g-°C
0.301 BTU/lb-°F
Thermal Conductivity 0.0330 - 0.0500 W/m-K
0.229 - 0.347 BTU-in/hr-ft²-°F
Melting Point 3499 °C
6330 °F