| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min; ASTM D790 |
|
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
PolyOne Trilliant™ HC HC3620-0040 RS Natural Polycarbonate + PBT (PC+PBT)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Network Polymers 779 Polystyrene
Description: Ignition RetardantInformation provided by Network Polymers Inc.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific)
ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM)
Information provided by Ravago
|
|||
| Flexural Modulus | 1.79 - 41.4 GPa | 260 - 6000 ksi | Average value: 12.3 GPa Grade Count:549 |
|
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Polymer Resources PC/TP-GP3 PC/Polyester Alloy
High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
|
|||
| Flexural Modulus | 1.79 - 3.43 GPa | 260 - 498 ksi | Average value: 2.87 GPa Grade Count:14 |
|
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Albis Plastics Cellulose Acetate Butyrate B930 (Base Grade), 4% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Albis Plastics Cellulose Acetate Butyrate B9304 (Odor Mask Added), 4% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | Tangent; ASTM D790 |
|
M. Holland Company PP700 Polypropylene Homopolymer
Features: Antistatic, NucleatedUses: Closure Caps, Thin-walled PartsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | |
|
Ineos Styrenics Avantra® 597N Polystyrene (NAFTA)
High-impact grade of polystyrene with improved impact strength and heat resistance, developed for injection molding and extrusion/thermoforming applications.Information provided by BASF.Ineos Styren..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE
A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE
A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Techmer ES HiFill® TPU GF40 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | Tangent; ASTM D790 |
|
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized
Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static)
Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Westlake Plastics PVDF Film Made from KYNAR® Polyvinylidene Fluoride Resin
Excellent chemical resistance. Stable to UV and the effects of weather. Low NBS smoke generation and superior LOI. Excellent transmittance of solar energy. Excellent dielectric strength. High h..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | 1.3mm per min, 1% secant; ASTM D790 |
|
Formosa Plastics Formolene® 4142T Injection Molding Polypropylene
Homopolymer with Nucleating, Antistat AdditivesApplications: Appliance, closure and thin wall applications.Formolene 4142T is a low viscosity, highly isotactic polypropylene homopolymer designed pri..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
American Polymers API 500 Polystyrene
API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 3716 Talc Filled Copolymer Polypropylene
DescriptionPolyfort® FPP 3716 is a 12% talc filled copolymer polypropylene product. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
CIP Composites 100 Series Laminated Polymer Bearing Material
The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated..
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Flexural Modulus | 1.79 GPa | 260 ksi | ASTM D790 |
|
LTL Color Compounds ColorRx™ PE3-0201A Antimicrobial LDPE
Low Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc.
|
|||