| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Novamid® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | DSM Novamid® 3010N 5-SL4-3X NAT PA66 FR.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.16 g/cc | 0.0419 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 2.70 % | 2.70 % | Sim. To ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 81.0 MPa | 11700 psi | dry; ISO 527-1/-2 |
| Elongation at Yield | 4.2 % | 4.2 % | dry; ISO 527-1/-2 |
| Tensile Modulus | 3.10 GPa | 450 ksi | dry; ISO 527-1/-2 |
| Flexural Strength | 65.0 MPa | 9430 psi | cond; ISO 178 |
| 125 MPa | 18100 psi | dry; ISO 178 | |
| Flexural Modulus | 1.60 GPa | 232 ksi | cond; ISO 178 |
| 3.40 GPa | 493 ksi | dry; ISO 178 | |
| Charpy Impact Unnotched | 12.3 J/cm² @Temperature 23.0 °C |
58.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
| NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
cond; ISO 179/1eU | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
| 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 260 °C | 500 °F | 10°C/min; ISO 11357-1/-3 |
| Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
dry; IEC 60695-11-10 |
| V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
dry; IEC 60695-11-10 |