Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Flexural Strength | <= 125 MPa | <= 18100 psi | ISO 178 |
Polykemi AB POLYfill PPH GF15030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178/1A |
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Nilit FRIANYL A63 KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178 |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Flexural Strength | 125 MPa | 18100 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 510 Polyethylene Terephthalate Application: friction bearings, wear linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU) Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D 790 |
SABIC Innovative Plastics Valox® AB9515 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay TECHNYL® A 217 PA66, DRY Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
SABIC Innovative Plastics NORYL NC212 PPE+HIPS (Asia Pacific) |
|||
Flexural Strength | 125 MPa | 18100 psi | ISO 178-93 |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790, ISO 178 |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Flexural Strength | 125 MPa | 18100 psi | |
Applied Nanostructured Solutions Carbon NanoStructure Encapsulated Flakes Carbon NanoStructure (CNS) Encapsulated Flakes are a unique form of carbon nanotubes, produced using a proprietary ANS process. The ANS process creates cross-linked multiwall carbon nanotube-based n.. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and .. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Flexural Strength | 125 MPa | 18100 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |
|||
Flexural Strength | 125 MPa | 18100 psi | 2 mm/min; ISO 178 |
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m.. |