Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 3.10 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Tensile Modulus 3.10 GPa
450 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/-2
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data)
Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c..
Tensile Modulus 3.10 GPa
450 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East)
LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
Tensile Modulus 3.10 GPa

@Temperature 23.0 °C
450 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66  (Unverified Data**)
Zytel® 103FHSA NC010 is a heat stabilized, lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 3.10 GPa
450 ksi
cond.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Spartech Polycast UF96 Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Modulus 3.10 GPa
450 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics NORYL PKN4752 PPE+PS (Europe-Africa-Middle East)
NORYL PKN4752 is a translucent, high heat PPO+PS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food cont..
Tensile Modulus 3.10 GPa
450 ksi
ASTM Test
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..
Tensile Modulus 3.10 GPa
450 ksi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-2
Total PSC 1340 Crystal Polystyrene
1340 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades such as LACQRENE® 7240. In dilution, LACQRENE® 1340 gives excellent pro..
Tensile Modulus >= 3.10 GPa
>= 450 ksi
Master Bond EP42HT-2FG Two Component Epoxy Adhesive for Food Applications
Master Bond Polymer System EP42HT-2FG is a room temperature setting, two component epoxy adhesive, sealant and coating specially formulated for food applications. It has been independently tested an..
Tensile Modulus 3.10 GPa
450 ksi
ASTM D638
Ensinger Delrin® 150 Homopolymer Acetal (POM)
Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g..
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/-2
DuPont Performance Polymers Delrin® PC650 NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC655 is a medium viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare..
Tensile Modulus 3.10 GPa
450 ksi
chs 0.2 in/min; ASTM D638
Diamond Polymers Centrex® 925 Injection Molding Grade
Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties..
Tensile Modulus 3.10 GPa
450 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by ..
Tensile Modulus 3.10 GPa
450 ksi
ISO 527-1/-2
Covestro Makroblend® DP 2-7655 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade
Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 10% mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new ..
Tensile Modulus 3.10 GPa
450 ksi
1mm/min; ISO 527
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Conditioned)
Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes..
Tensile Modulus 3.10 GPa
450 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont..
Tensile Modulus 3.10 GPa
450 ksi
TM R050-36
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin
Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1..
Tensile Modulus 3.10 GPa
450 ksi
ASTM D-638
Axiall 5006 Rigid PVC, Extrusion, White
Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia G..
Tensile Modulus 3.10 GPa
450 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics SABIC PPCOMPOUND 15T1020 PP
SABIC® PPcompound 15T1020. This grade is a general purpose, talc filled, heat stabilized polypropylene resin suitable for injection molded applications. The IMDS ID is 16486973.
Tensile Modulus 3.10 GPa
450 ksi
TM R050-36
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett..
Copyright © lookpolymers.com All Rights Reserved