| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 77 | 77 | Conditioned; ISO 868 |
| 83 | 83 | ISO 868 | |
| Tensile Strength at Break | 120 MPa | 17400 psi | Conditioned; ISO R 527 |
| 195 MPa | 28300 psi | ISO R 527 | |
| Elongation at Yield | 2.0 % | 2.0 % | ISO R 527 |
| 4.0 % | 4.0 % | Conditioned; ISO R 527 | |
| Modulus of Elasticity | 6.20 GPa | 899 ksi | Conditioned; ISO 178 |
| 11.0 GPa | 1600 ksi | ISO 178 | |
| Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1A |
| 23.0 kJ/m² | 10.9 ft-lb/in² | Conditioned; ISO 180/1A | |
| Charpy Impact Unnotched | 6.50 J/cm² | 30.9 ft-lb/in² | ISO 179/IeU |
| 7.50 J/cm² | 35.7 ft-lb/in² | Conditioned; ISO 179/IeU | |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/IeA |
| 1.90 J/cm² | 9.04 ft-lb/in² | Conditioned; ISO 179/IeA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 25.0 µm/m-°C | 13.9 µin/in-°F | ASTM E831 |
| Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | ISO 75-2/AF |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
| 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | Conditioned; CEI 60243-1 |
| 35.0 kV/mm | 889 kV/in | CEI 60243-1 | |
| Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |