Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced |
Manufacturer | Addiplast |
Trade Name | Addinyl |
Port | Ningbo port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Addiplast Addinyl PMD 20170 Nylon 66.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.46 g/cc | 0.0527 lb/in³ | ISO 1183/A |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore D | 84 | 84 | Conditioned; ISO 868 |
88 | 88 | ISO 868 | |
Tensile Strength at Break | 60.0 MPa | 8700 psi | Conditioned; ISO R 527 |
85.0 MPa | 12300 psi | ISO R 527 | |
Elongation at Yield | 5.0 % | 5.0 % | ISO R 527 |
25 % | 25 % | Conditioned; ISO R 527 | |
Modulus of Elasticity | 1.60 GPa | 232 ksi | Conditioned; ISO 178 |
5.00 GPa | 725 ksi | ISO 178 | |
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1A |
9.00 kJ/m² | 4.28 ft-lb/in² | Conditioned; ISO 180/1A | |
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/IeU |
NB | NB | Conditioned; ISO 179/IeU | |
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
0.900 J/cm² | 4.28 ft-lb/in² | Conditioned; ISO 179/IeA |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 µm/m-°C | 30.6 µin/in-°F | ASTM E831 |
Melting Point | 260 °C | 500 °F | ISO 3146/C2 |
Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | ISO 75-2/AF |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | Conditioned; CEI 60093 |
1.00e+15 ohm-cm | 1.00e+15 ohm-cm | CEI 60093 | |
Comparative Tracking Index | 550 V | 550 V | CEI 60112/Solution A |