PRODUCT NO. Category Trade Name
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded Melamine-Phenolic Copolymer
Plenco 00755 Melamine-Phenolic, Granular, Transfer Molded Melamine-Phenolic Copolymer
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded Melamine-Phenolic Copolymer
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded Melamine-Phenolic Copolymer
Plenco 08122 Polyester BMC, Compression Molded Thermoset Polyester Glass Filled BMC
Plenco 08133 Polyester BMC, Compression Molded Thermoset Polyester Glass Filled BMC
Plenco 08218 Polyester BMC, Compression Molded Thermoset Polyester Glass Filled BMC
Plenco 08235 Polyester BMC, Compression Molded Thermoset Polyester Glass Filled BMC
Plenco 1500 Polyester, Granular, Compression Molded Thermoset Polyester, Mineral Filled
Plenco 1508 Polyester, Briquette, Injection Molded Thermoset Polyester, Mineral Filled
Plenco 1508 Polyester, Briquette, Transfer Molded Thermoset Polyester, Mineral Filled
Plenco 1530 Polyester, Briquette, Injection Molded Thermoset Polyester Glass and Mineral Filled BMC
Plenco 1581 Polyester, Pellet, Injection Molded Thermoset Polyester Glass and Mineral Filled BMC
Plenco 1586 Polyester, Pellet, Injection Molded Thermoset Polyester Glass and Mineral Filled BMC
Plenco 2000 Phenolic, Granular, Compression Molded Phenolic, Novolac, Woodflour Filled
Plenco 2308 Phenolic, Granular, Compression Molded Phenolic, Novolac, Woodflour Filled
Plenco 2369 Phenolic, Granular, Compression Molded Phenolic, Resole, Wood Filled
Plenco 2369 Phenolic, Granular, Transfer Molded Phenolic, Resole, Wood Filled
Plenco 2535 Phenolic, Granular, Injection Molded Phenolic, Novolac, Woodflour Filled
Plenco 3356 Phenolic, Granular, Compression Molded Phenolic, Novolac, Mineral Filled
Plenco 3356 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Mineral Filled
Plenco 3509 Phenolic, Granular, Injection Molded Phenolic, Novolac, Mineral/Flock Filled
Plenco 3509 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Mineral/Flock Filled
Plenco 4349 Phenolic, Granular, Compression Molded Phenolic, Novolac, Mineral Filled
Plenco 4349 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Mineral Filled
Plenco 4527 Phenolic, Granular, Transfer Molded Phenolic, Resole, Mineral/Flock Filled
Plenco 4548 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Mineral Filled
Plenco 4599 Phenolic, Granular, Injection Molded Phenolic, Novolac, Mineral Filled
Plenco 5118 Phenolic, Granular, Compression Molded Phenolic, Novolac, Mineral/Graphite Filled
Plenco 5118 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Mineral/Graphite Filled
Plenco 6015 Phenolic, Briquette, Transfer Molded Phenolic, Novolac, Mineral/Glass Filled
Plenco 6553 Phenolic, Granular, Compression Molded Phenolic; Unreinforced; Molded
Plenco 6990 Phenolic, Briquette, Transfer Molded Phenolic, Novolac, Mineral/Glass Filled
Plenco 7100 Phenolic, Nodular, Injection Molded Phenolic, Novolac, Flock Filled
Plenco 7200 Phenolic, Granular, Transfer Molded Phenolic
Plenco 7500 Phenolic, Granular, Injection Molded Phenolic, Novolac, Woodflour Filled
Plenco 7500 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Woodflour Filled
Plenco 7507 Phenolic, Granular, Compression Molded Phenolic, Resole, Wood Filled
Plenco 2408 Phenolic, Granular, Injection Molded Phenolic, Resole, Wood Filled
Plenco 4309 Phenolic, Nodular, Injection Molded Phenolic, Novolac, Glass Filled
Plenco 4311 Phenolic, Granular, Compression Molded Phenolic, Novolac, Mineral Filled
Plenco 4311 Phenolic, Granular, Injection Molded Phenolic, Novolac, Mineral Filled
Plenco 5350 Phenolic, Granular, Compression Molded Phenolic, Novolac, Mineral/Graphite Filled
Plenco 1581 Polyester, Briquette, Transfer Molded Thermoset Polyester Glass and Mineral Filled BMC
Plenco 2000 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Woodflour Filled
Plenco 2311 Phenolic, Granular, Transfer Molded Phenolic, Novolac, Woodflour Filled
Plenco 7321 Phenolic, Nodular, Injection Molded Phenolic, Novolac, Flock Filled
Plenco 7591 Phenolic, Pellet, Transfer Molded Phenolic, Novolac, Mineral/Flock Filled
Plenco 7697 Phenolic, Granular, Compression Molded Phenolic, Novolac, Impact Grade, Filled