Category : Phenolic, Novolac, Woodflour Filled Product List

Tips: 50 items are displayed at most. For the rest of the results, please contact customer service.
PRODUCT NO. Manufacturer Trade Name
Overview of materials for Phenolic, Novolac, Woodflour Filled
Plenco 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok 202 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plenco 2000 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2000 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 2300 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2308 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2308 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 2308 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 2311 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2311 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 2482 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 2535 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2535 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 2571 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 2571 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 3554 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 5482 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 5482 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 7500 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 7500 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 7500 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 2300 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 2571 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plenco 2000 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 2311 Phenolic, Granular, Transfer Molded Plenco (Plastics Engineering Company)
Plenco 7579 Phenolic, Granular, Compression Molded Plenco (Plastics Engineering Company)
Plenco 7579 Phenolic, Granular, Injection Molded Plenco (Plastics Engineering Company)
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)