Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 00757 Melamine-Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Plenco 00757 Melamine-Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00757 is available only in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Water Absorption 0.285 %
0.285 %
ASTM D570
Linear Mold Shrinkage 0.0057 cm/cm
0.0057 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 67
67
ASTM D785
Tensile Strength, Ultimate 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 11.8 GPa
1710 ksi
ASTM D638
Flexural Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 9.90 GPa
1440 ksi
ASTM D790
Compressive Strength 142 MPa
20600 psi
ASTM D695
Izod Impact, Notched 0.205 J/cm
0.384 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.217 J/cm²
1.03 ft-lb/in²
ASTM D256
Impact 132
132
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.610 W/m-K

@Temperature 100 °C
4.23 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 144 °C
291 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
Oxygen Index 36 %
36 %
ASTM D2863
Shrinkage 0.95 %
0.95 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.30e+11 ohm-cm
6.30e+11 ohm-cm
ASTM D247
Dielectric Constant 7.6
7.6
ASTM D150
Dielectric Strength 5.50 kV/mm
140 kV/in
Step by Step; ASTM D149
7.80 kV/mm
198 kV/in
Short Time; ASTM D149
Dissipation Factor 0.114
0.114
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved