Material Notes:
PLENCO 03509 is a mineral and flock filled phenolic molding compound offering excellent electrical properties, dimensional stability, and improved heat resistance. UL recognized under component file E40654. 03509 is available in black or brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
ASTM D1895
Density 1.57 g/cc
0.0567 lb/in³
ASTM D792
Water Absorption 0.202 %
0.202 %
ASTM D570
Linear Mold Shrinkage 0.0064 cm/cm
0.0064 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 81
81
ASTM D785
Tensile Strength, Ultimate 53.0 MPa
7690 psi
ASTM D638
Elongation at Break 0.97 %
0.97 %
ASTM D638
Tensile Modulus 8.50 GPa
1230 ksi
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 8.40 GPa
1220 ksi
ASTM D790
Compressive Strength 181 MPa
26300 psi
ASTM D695
Poissons Ratio 0.33
0.33
ASTM D638
Shear Modulus 3.20 GPa
464 ksi
Calculated
Izod Impact, Notched 0.170 J/cm
0.318 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.195 J/cm²
0.928 ft-lb/in²
ASTM D256
Impact 118
118
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C

@Temperature 40.0 - 130 °C
27.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.450 W/m-K

@Temperature 100 °C
3.12 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 197 °C
387 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
360 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 36 %
36 %
ASTM D2863
Shrinkage 0.238 %
0.238 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.60e+11 ohm-cm
3.60e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 8.50 kV/mm
216 kV/in
Step by Step; ASTM D149
12.8 kV/mm
325 kV/in
Short Time; ASTM D149
Dissipation Factor 0.052
0.052
ASTM D150
Arc Resistance 168 sec
168 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638