Material Notes:
PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorption, and excellent dimensional stability under severe exposure. 05118 is available in gray. 05118 is not recommended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.870 g/cc
0.0314 lb/in³
ASTM D1895
Density 1.81 g/cc
0.0654 lb/in³
ASTM D792
Water Absorption 0.045 %
0.045 %
ASTM D570
Linear Mold Shrinkage 0.00173 cm/cm
0.00173 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 59
59
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 0.58 %
0.58 %
ASTM D638
Tensile Modulus 12.9 GPa
1870 ksi
ASTM D638
Flexural Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 11.1 GPa
1610 ksi
ASTM D790
Compressive Strength 144 MPa
20900 psi
ASTM D695
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.193 J/cm²
0.919 ft-lb/in²
ASTM D256
Impact 63
63
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
378 °F
ASTM D648
Shrinkage 0.044 %
0.044 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.20e+11 ohm-cm
4.20e+11 ohm-cm
ASTM D247
Dielectric Constant 18.6
18.6
ASTM D150
Dissipation Factor 0.051
0.051
ASTM D150
Comparative Tracking Index 300 V
300 V
ASTM D3638