Plenco 2535 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2535 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 02535 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.41 %
0.41 %
ASTM D570
Linear Mold Shrinkage 0.0107 cm/cm
0.0107 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 85
85
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.83 %
0.83 %
ASTM D638
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Flexural Strength 81.0 MPa
11700 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Compressive Strength 202 MPa
29300 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.87 GPa
416 ksi
Calculated
Izod Impact, Notched 0.186 J/cm
0.348 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.186 J/cm²
0.885 ft-lb/in²
ASTM D256
Impact 103
103
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 43.0 µm/m-°C

@Temperature 40.0 - 130 °C
23.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 196 °C
385 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 26.1 %
26.1 %
ASTM D2863
Shrinkage 0.44 %
0.44 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+11 ohm-cm
2.30e+11 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 10.2 kV/mm
259 kV/in
Short Time; ASTM D149
Dissipation Factor 0.057
0.057
ASTM D150
Arc Resistance 126 sec
126 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638