Material Notes:
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component file E40654. 07500 is available in black or red color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 90
90
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.78 %
0.78 %
ASTM D638
Tensile Modulus 7.70 GPa
1120 ksi
ASTM D638
Flexural Strength 81.0 MPa
11700 psi
ASTM D790
Flexural Modulus 7.40 GPa
1070 ksi
ASTM D790
Compressive Strength 218 MPa
31600 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.83 GPa
410 ksi
Calculated
Izod Impact, Notched 0.204 J/cm
0.382 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.206 J/cm²
0.980 ft-lb/in²
ASTM D256
Impact 119
119
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 58.0 µm/m-°C

@Temperature 40.0 - 130 °C
32.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 200 °C
392 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
331 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 24.7 %
24.7 %
ASTM D2863
Shrinkage 0.253 %
0.253 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.90e+11 ohm-cm
3.90e+11 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 11.1 kV/mm
282 kV/in
Short Time; ASTM D149
Dissipation Factor 0.051
0.051
ASTM D150
Arc Resistance 128 sec
128 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638