Plenco 2000 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2000 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under component file E40654. 02000 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.630 g/cc
0.0228 lb/in³
ASTM D1895
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Linear Mold Shrinkage 0.0044 cm/cm
0.0044 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 90
90
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.65 %
0.65 %
ASTM D638
Tensile Modulus 8.60 GPa
1250 ksi
ASTM D638
Flexural Strength 92.0 MPa
13300 psi
ASTM D790
Flexural Modulus 8.10 GPa
1170 ksi
ASTM D790
Compressive Strength 212 MPa
30700 psi
ASTM D695
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.187 J/cm²
0.890 ft-lb/in²
ASTM D256
Impact 109
109
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 59.0 µm/m-°C

@Temperature 40.0 - 130 °C
32.8 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.390 W/m-K

@Temperature 100 °C
2.71 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 207 °C
405 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 27.9 %
27.9 %
ASTM D2863
Shrinkage 0.203 %
0.203 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.20e+11 ohm-cm
3.20e+11 ohm-cm
ASTM D247
Dielectric Constant 5.2
5.2
ASTM D150
Dielectric Strength 12.2 kV/mm
310 kV/in
Short Time; ASTM D149
Dissipation Factor 0.052
0.052
ASTM D150
Arc Resistance 132 sec
132 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638