Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
|
Iran Petrochemical (PCC) 12XF6 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) 16503 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Film Grade |
|
Iran Petrochemical (PCC) 2100TN00 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 2102TX00 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 2501TN00 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 5218EA High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 52511 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 52518 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 52528 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 6040UA High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 60505 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) Arak BL6 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak I2 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak I4 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) BL 4M HM 8355 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL4 HM 8255 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL5 HM 7746 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) EX 1 HF 7740F High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) EX 2 HF 7750 M High Density Polyethylene |
HDPE, Fiber Grade |
|
Iran Petrochemical (PCC) EX 2 S HF 7750 M2 High Density Polyethylene |
HDPE, Fiber Grade |
|
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene |
High Density Polyethylene (HDPE), Pipe Grade |
|
Iran Petrochemical (PCC) EX 4 HM9455 F High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) HB0035 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) HB4265 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) HB5020 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) I1 HA 7260 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) I4 HD 7255 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LH0030 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LL 18XF5 N Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) LL0209 SR Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
|
Iran Petrochemical (PCC) LL0220KJ Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
|
Iran Petrochemical (PCC) LS0085 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) MF3313 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) MF3713 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) 1922T Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
|
Iran Petrochemical (PCC) 2004TC37 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) 235F7 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene |
Medium Density Polyethylene (MDPE), Rotational Molded |
|
Iran Petrochemical (PCC) 5030UA High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 60507 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 6070EA High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) 7000F High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) Arak BL2 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak BL3 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak BL4 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak BL5 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak EX3 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) Arak I3 HDPE |
High Density Polyethylene (HDPE), Injection Molded |
Arak
|
Iran Petrochemical (PCC) BL 3VD HH 4765 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) BL7 HM 6255 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene |
HDPE, Fiber Grade |
|
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene |
High Density Polyethylene (HDPE), Pipe Grade |
|
Iran Petrochemical (PCC) EX 4HS HM 9455 F1 High Density Polyethylene |
High Density Polyethylene (HDPE), Film Grade |
|
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene |
High Density Polyethylene (HDPE), Pipe Grade |
|
Iran Petrochemical (PCC) EX7C HF4750K High Density Polyethylene |
High Density Polyethylene (HDPE), Extruded |
|
Iran Petrochemical (PCC) HB5510 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) I2 HB 7250 High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) I3 HC 7260(THE) High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) I3S HC 7260(THE) High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
|
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LF0250/KJ Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LL0209 KJ Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
|
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
|
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE)/Butene, Film |
|
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene |
Linear Low Density Polyethylene (LLDPE), Blow Molding Grade |
|
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene |
Low Density Polyethylene (LDPE), Film Grade |
|
Iran Petrochemical (PCC) MF3820 High Density Polyethylene |
High Density Polyethylene (HDPE), Blow Molding Grade |
|