Iran Petrochemical (PCC) HB4265 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) HB4265 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HB4265 is a high molecular weight high density polyethylene.Applications: tanks, industrial, blow molding.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.942 g/cc
0.0340 lb/in³
ISO 1183
Melt Flow 6.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Impact Strength 160 kJ/m²

@Temperature -30.0 °C
76.1 ft-lb/in²

@Temperature -22.0 °F
ISO 8256