Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Iran Petrochemical (PCC) EX 2 HF 7750 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EX2 (HF 7750) is high density polyethylene with propylene as co monomer. It has a medium molar mass with a narrow molar mass distribution.Application: production of monofilaments with high tensile strength.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 2.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
27 g/10 min

@Load 21.6 kg,
Temperature 190 °C
27 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Processing Properties Metric English Comments
Melt Temperature 200 - 230 °C
392 - 446 °F
Descriptive Properties Value Comments
Gel Number <5
Internal Test Method
Gels Size <150 µm
Internal Test Method