| Huntsman AVALON® 550 B Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 80 ABU Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 80 ABX Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 95 AHT DP Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman IROGRAN® A 75 P 4665N TPU-Polyether |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 78 P 4766 TPU-Polyether |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 80 P 5039 TPU-Polyether |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 85 E 4719 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 85 E 4993 FCM Polyester-Based TPU-Injection Extrusion Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 85 H 4508 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 85 P 4350 TPU-Polyether |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 85 P 4394 UV TPU-Polyether |
Thermoplastic Polyurethane (TPUR), Polyether Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 85 P 5004 TPU-Polyether |
Thermoplastic Polyurethane (TPUR), Polyether Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 86 E 4486 Polyester-Based TPU-Injection Extrusion Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 95 E 4813 Polyester-Based TPU-High Performance Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 95 E 4861 Polyester-Based TPU-Injection Extrusion Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 98 P 4535 TPU-Polyether |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® D 64 P 4777 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS 370-202 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS 440-200 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS 455-204 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS 456-202 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS442-202 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS455-200 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® PS455-203 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film |
Film |
KRYSTALFLEX®
|
| Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film |
Film |
KRYSTALFLEX®
|
| Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film |
Film |
KRYSTALFLEX®
|
| Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film |
Film |
KRYSTALFLEX®
|
| Huntsman AVALON® 65 ABX Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 65 AE Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 65 AK Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 65 DB Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 65 DE Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 75 AE Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 85 ABX Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 85 AE Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 90 AKU Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 92 AB Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman AVALON® 95 AEU Thermoplastic Polyurethane |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
Avalon®
|
| Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 85 P 4854 Ether-Based TPU-For Cable Industry |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade |
Polyurethane TPE |
IROGRAN®
|
| Huntsman IROGRAN® A 92 E 4860 TPU-Polyester |
Thermoplastic Polyurethane (TPUR), Polyester Grade |
IROGRAN®
|
| Huntsman IROGRAN® A 92 K 4107 TPU-High Temperature Performance |
Polyurethane TPE |
IROGRAN®
|