Huntsman IROGRAN® CA 117-200 DP TPU-Polyester

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® CA 117-200 DP TPU-Polyester.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polyester-based TPUs that are specially designed for adhesives applications where high green strength and a fast crystallization rate are essential qualities.Information provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Hardness, Shore D 49
49
ASTM D2240
Tensile Strength at Break 19.1 MPa
2770 psi
ASTM D412
Elongation at Break 660 %
660 %
ASTM D412
50% Modulus 0.00607 GPa
0.880 ksi
ASTM D412
100% Modulus 0.00627 GPa
0.910 ksi
ASTM D412
300% Modulus 0.00689 GPa
1.00 ksi
ASTM D412
Rebound 44 %
44 %
Bayshore; ASTM D2632
Tear Strength 92.9 kN/m
530 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 108
108
ASTM D3389
Thermal Properties Metric English Comments
Melting Point 71.0 - 93.0 °C
160 - 199 °F
TMA Melt Range
Vicat Softening Point 46.0 °C
115 °F
ASTM D1525
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
Midpoint; ASTM E 1269