Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 38.0 kV/mm @Thickness 2.00 mm |
965 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LAXTAR G/30 30% Glass Reinforced LCP
(discontinued **) Description: Laxtar products are liquid crystal polymers (LCP). They offer exceptional performance together with increasing cost-effectiveness. Due to the outstanding fluidity at high shear rates LC.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Ineos ABS Lustran® H801 High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers PA 66, 15% glass fibers, injection molding, heat-ageing stabilized |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | IEC 60243-1 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Milled Glass Fiber PA 6, injection molding grade, 30% milled fibers, UL 94V-2 at 0.8 mm, max. temperature in glow wire test: 960 °C at 0,75 mm, "halogen-free", good heat-ageing resistanceApplication Examples: Medic.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S KR 2864 C UV Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-15H PA6T/66-GF15 Product description: Grivory HT2V-15H is a 15 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3H PA6T/66-GF30 Product description: Grivory HT2V-3H is a 30 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamde. Polymer designation acc. to ISO: .. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50 Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33 Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | IEC 60243-1 |
DuPont Performance Polymers Rynite® 940 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
ASTM D149 |
Arkema Group Orgalloy® R 60 ES Polyamide Alloy Polyamide Alloy, Film and PackagingInformation provided by Arkema Group |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Dielectric Strength | 38.0 kV/mm @Thickness 1.00 mm |
965 kV/in @Thickness 0.0394 in |
ASTM D149 |
Arkema Group Orgalloy® RS 60E10 Polyamide Alloy Polyamide Alloy, Rigid Blown film gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 6000TLA Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S KR 2861/1 C Colored ASA+PC Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh.. |
|||
Dielectric Strength | 38.0 kV/mm | 965 kV/in | |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |