Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.0 - 25.0 kV/mm | 508 - 635 kV/in | IEC 60243-1 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm | 508 - 635 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm | 508 - 635 kV/in | IEC 60243-1 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Dielectric Strength | 24.0 - 25.0 kV/mm | 610 - 635 kV/in | Average value: 24.3 kV/mm Grade Count:3 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 16.7 - 25.0 kV/mm | 425 - 635 kV/in | Average value: 19.6 kV/mm Grade Count:7 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 7.00 - 25.0 kV/mm | 178 - 635 kV/in | Average value: 11.2 kV/mm Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Dielectric Strength | 11.0 - 25.0 kV/mm | 279 - 635 kV/in | Average value: 21.0 kV/mm Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS); Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS); Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Strength | 15.7 - 25.0 kV/mm | 400 - 635 kV/in | Average value: 19.6 kV/mm Grade Count:6 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm | 508 - 635 kV/in | ASTM D149 |
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Features: Copolymer; Good Flexibility; Medium ViscosityAdditional Properties: Crystal.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm |
508 - 635 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Dielectric Strength | 15.0 - 25.0 kV/mm | 381 - 635 kV/in | DC Breakdown Strength |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 16.0 - 25.0 kV/mm | 406 - 635 kV/in | DIN 53481 |
Isoflon PA 6 Polyamide 6 General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon. |
|||
Dielectric Strength | 23.0 - 25.0 kV/mm | 584 - 635 kV/in | DIN 53481 |
Isoflon PAI Polyamideimide Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon. |
|||
Dielectric Strength | 19.7 - 25.0 kV/mm | 500 - 635 kV/in | Average value: 21.1 kV/mm Grade Count:11 |
Overview of materials for Polypropylene with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i.. |
|||
Dielectric Strength | 2.60 - 25.0 kV/mm | 66.0 - 635 kV/in | Average value: 23.1 kV/mm Grade Count:51 |
Overview of materials for Thermoset Fluoroelastomer This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr.. |