Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HH120 Anaerobic Threadlocker Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond LH197 Anaerobic Gasketmaker Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond LM113 Anaerobic Threadlocker Permabond® LM113 Threadlocker is a medium viscosity product for locking small threaded fasteners, such as screws and bolts or hydraulic fittings that might require disassembly. Due to its thixotrop.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HH040 Anaerobic Retainer Permabond® HH040 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure unitiz.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MH199 Anaerobic Gasketmaker Permabond® MH199 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Dielectric Strength | 11.0 - 70.0 kV/mm | 280 - 1780 kV/in | Average value: 27.9 kV/mm Grade Count:55 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 85Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | JIS-K-6249; ASTM D-149 |
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p.. |
|||
Dielectric Strength | 11.0 kV/mm | 280 kV/in | short time 2 mm thick; ASTM D149 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | Short Time; ASTM D149 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149; at 1 mil |
Westlake Plastics HTP 800 Clear PVC HTP 800 is a clear PVC based material for use as windows and doors in cleanroom equipment. Notable properties include light transmission, chemical resistance, and flame resistance. Information prov.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
279 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Dielectric Strength | 11.0 kV/mm @Thickness 3.00 mm |
279 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola G-Etronax EP 22 Epoxy, Glass Fabric Reinforcement, Light Yellow, Tubes Description: Particularly good electrical and mechanical properties. Extremely high mechanical strength, even at high temperatures. Retains electrical properties at high air humidity. High resistanc.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A1042 Anaerobic Threadlocker Permabond® A1042 is a rapid curing adhesive designed to lock and seal metal parts that subsequently may need to be dismantled for maintenance. The high vibration resistance makes Permabond A1042 pa.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A1044 Anaerobic Threadsealant Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | ASTM D149 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A1046 Anaerobic Retainer Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and .. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |
|||
Dielectric Strength | 11.0 kV/mm | 279 kV/in | |
Permabond A136 Anaerobic Gasketmaker Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent.. |