Overview of materials for Thermoset Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Thermoset Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 3.80 g/cc
0.0325 - 0.137 lb/in³
Average value: 1.85 g/cc Grade Count:257
Oxygen Transmission 88.0 - 150 cc-mm/m²-24hr-atm
224 - 381 cc-mil/100 in²-24hr-atm
Average value: 104 cc-mm/m²-24hr-atm Grade Count:42
Mooney Viscosity 3.00 - 200
3.00 - 200
Average value: 53.2 Grade Count:312
Mechanical Properties Metric English Comments
Hardness, Shore A 38.0 - 100
38.0 - 100
Average value: 73.5 Grade Count:613
35.0 - 85.0

@Temperature 225 - 225 °C
35.0 - 85.0

@Temperature 437 - 437 °F
Average value: 86.0 Grade Count:1
58.0 - 98.0

@Temperature 93.3 - 200 °C
58.0 - 98.0

@Temperature 200 - 392 °F
Average value: 86.0 Grade Count:11
58.0 - 98.0

@Time 252000 - 3.60e+6 sec
58.0 - 98.0

@Time 70.0 - 1000 hour
Average value: 86.0 Grade Count:11
Hardness, Shore D 47.0 - 80.0
47.0 - 80.0
Average value: 59.8 Grade Count:4
Hardness, Shore M 72.0 - 83.0
72.0 - 83.0
Average value: 78.5 Grade Count:11
Tensile Strength, Ultimate 0.750 - 130 MPa
109 - 18900 psi
Average value: 13.4 MPa Grade Count:541
17.24 - 20.68 MPa

@Temperature 225 - 225 °C
2500 - 2999 psi

@Temperature 437 - 437 °F
Average value: 17.8 MPa Grade Count:1
8.40471 - 25.7933 MPa

@Temperature 93.3 - 275 °C
1219.00 - 3741.01 psi

@Temperature 200 - 527 °F
Average value: 17.8 MPa Grade Count:16
8.40471 - 25.7933 MPa

@Time 86400 - 3.60e+6 sec
1219.00 - 3741.01 psi

@Time 24.0 - 1000 hour
Average value: 17.8 MPa Grade Count:16
Tensile Strength, Yield 0.300 - 23.0 MPa
43.5 - 3340 psi
Average value: 6.03 MPa Grade Count:570
Elongation at Break 3.10 - 500 %
3.10 - 500 %
Average value: 217 % Grade Count:640
150 - 160 %

@Temperature 225 - 225 °C
150 - 160 %

@Temperature 437 - 437 °F
Average value: 196 % Grade Count:1
61.6 - 456.5 %

@Temperature 93.3 - 275 °C
61.6 - 456.5 %

@Temperature 200 - 527 °F
Average value: 196 % Grade Count:16
61.6 - 456.5 %

@Time 86400 - 3.60e+6 sec
61.6 - 456.5 %

@Time 24.0 - 1000 hour
Average value: 196 % Grade Count:16
Modulus of Elasticity 0.000600 - 9.20 GPa
0.0870 - 1330 ksi
Average value: 0.234 GPa Grade Count:42
Compressive Modulus 0.000300 - 0.0153 GPa
0.0435 - 2.22 ksi
Average value: 0.00534 GPa Grade Count:4
Shear Modulus 0.00193 - 0.0243 GPa
0.280 - 3.53 ksi
Average value: 0.00760 GPa Grade Count:19
0.0430 - 0.0430 GPa

@Temperature -12.0 - -12.0 °C
6.24 - 6.24 ksi

@Temperature 10.4 - 10.4 °F
Average value: 0.0430 GPa Grade Count:2
Secant Modulus 0.00512 - 0.0685 GPa
0.743 - 9.94 ksi
Average value: 0.0215 GPa Grade Count:19
Coefficient of Friction 0.500 - 1.16
0.500 - 1.16
Average value: 0.791 Grade Count:51
Tear Strength Test 132 - 359
132 - 359
Average value: 232 Grade Count:21
Tear Strength 3.06 - 168 kN/m
17.5 - 959 pli
Average value: 24.5 kN/m Grade Count:89
5.20 - 10.4 kN/m

@Temperature 150 - 150 °C
29.7 - 59.3 pli

@Temperature 302 - 302 °F
Average value: 8.16 kN/m Grade Count:5
Taber Abrasion, mg/1000 Cycles 40.0 - 325
40.0 - 325
Average value: 184 Grade Count:5
Compression Set 3.00 - 69.0 %
3.00 - 69.0 %
Average value: 22.0 % Grade Count:264
4.00 - 65.0 %

@Temperature 100 - 300 °C
4.00 - 65.0 %

@Temperature 212 - 572 °F
Average value: 24.0 % Grade Count:266
4.00 - 91.0 %

@Temperature 0.000 - 325 °C
4.00 - 91.0 %

@Temperature 32.0 - 617 °F
Average value: 24.0 % Grade Count:237
4.00 - 91.0 %

@Time 79200 - 2.42e+6 sec
4.00 - 91.0 %

@Time 22.0 - 672 hour
Average value: 24.0 % Grade Count:237
Thermal Properties Metric English Comments
CTE, linear 19.0 - 570 µm/m-°C
10.6 - 317 µin/in-°F
Average value: 223 µm/m-°C Grade Count:49
Specific Heat Capacity 1.65 - 1.67 J/g-°C
0.394 - 0.399 BTU/lb-°F
Average value: 1.65 J/g-°C Grade Count:40
0.945 - 1.053 J/g-°C

@Temperature 50.0 - 150 °C
0.226 - 0.2517 BTU/lb-°F

@Temperature 122 - 302 °F
Average value: 0.991 J/g-°C Grade Count:4
Thermal Conductivity 0.200 - 0.300 W/m-K
1.39 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.235 W/m-K Grade Count:40
0.170 - 0.190 W/m-K

@Temperature 50.0 - 200 °C
1.18 - 1.32 BTU-in/hr-ft²-°F

@Temperature 122 - 392 °F
Average value: 0.180 W/m-K Grade Count:4
Maximum Service Temperature, Air 93.3 - 350 °C
200 - 662 °F
Average value: 235 °C Grade Count:298
Minimum Service Temperature, Air -65.0 - 2.22 °C
-85.0 - 36.0 °F
Average value: -20.0 °C Grade Count:299
Brittleness Temperature -60.0 - -6.00 °C
-76.0 - 21.2 °F
Average value: -24.6 °C Grade Count:100
Glass Transition Temp, Tg -51.1 - 3.00 °C
-60.0 - 37.4 °F
Average value: -18.6 °C Grade Count:174
Transformation Temperature -40.0 - -2.00 °C
-40.0 - 28.4 °F
Average value: -8.54 °C Grade Count:13
Flash Point 15.6 - 400 °C
60.1 - 752 °F
Average value: 323 °C Grade Count:93
Optical Properties Metric English Comments
Transmission, Visible 25.0 - 90.0 %
25.0 - 90.0 %
Average value: 35.8 % Grade Count:6
Component Elements Properties Metric English Comments
Fluorine, F 64.0 - 73.0 %
64.0 - 73.0 %
Average value: 67.4 % Grade Count:66
Electrical Properties Metric English Comments
Electrical Resistivity 0.00500 - 5.00e+17 ohm-cm
0.00500 - 5.00e+17 ohm-cm
Average value: 4.06e+16 ohm-cm Grade Count:53
Shielding Effectiveness 70.0 - 113 dB
70.0 - 113 dB
Average value: 98.3 dB Grade Count:3
Dielectric Constant 2.50 - 11.4
2.50 - 11.4
Average value: 9.80 Grade Count:44
Dielectric Strength 2.60 - 25.0 kV/mm
66.0 - 635 kV/in
Average value: 23.1 kV/mm Grade Count:51
Dissipation Factor 0.00500
0.00500
Average value: 0.00500 Grade Count:4
Processing Properties Metric English Comments
Processing Temperature 160 - 260 °C
320 - 500 °F
Average value: 201 °C Grade Count:170
Die Temperature 70.0 - 260 °C
158 - 500 °F
Average value: 138 °C Grade Count:3
Cure Time 1.50 - 4320 min
0.0250 - 72.0 hour
Average value: 324 min Grade Count:27
10.0 - 10.0 min

@Temperature 121 - 121 °C
0.167 - 0.167 hour

@Temperature 250 - 250 °F
Average value: 10.0 min Grade Count:2