| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
|
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive
Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature..
|
|||
| Dielectric Strength | 15.7 - 200 kV/mm | 400 - 5080 kV/in | Average value: 35.4 kV/mm Grade Count:30 |
|
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
|
|||
| Dielectric Strength |
15.7
kV/mm @Thickness 3.17 mm |
400
kV/in @Thickness 0.125 in |
|
|
Ineos Nova 5751 High Impact Polystyrene
(discontinued **)
High flow, Good impact, USP Class VIApplications: Single service impact, Medical, Housewares, CompoundingProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwi..
|
|||
| Dielectric Strength | 15.7 - 35.0 kV/mm | 400 - 889 kV/in | Average value: 27.6 kV/mm Grade Count:10 |
|
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 515880R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wr..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
|
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
|
Techmer ES HiFill® PA6 GF20 L BK001 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Additive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 8376102Information provid..
|
|||
| Dielectric Strength |
15.7
kV/mm @Thickness 3.17 mm |
400
kV/in @Thickness 0.125 in |
|
|
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy
Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
|
Tra-Con Tra-Bond F123LV Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F123LV is a fast cure, low viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating s..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
|
Tra-Con Tra-Bond F123MV Color Keyed High Temperature Epoxy Adhesive
TRA-BOND F123 MV is a fast cure, medium viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminati..
|
|||
| Dielectric Strength |
15.7
-
17.7
kV/mm @Thickness 3.17 mm |
400
-
450
kV/in @Thickness 0.125 in |
Short time value |
|
Abatron AboCast/AboCure 8109-13
Liquid hardener version of AboCast/AboCure 8109-11.Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | ASTM D149 |
|
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier
Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 920-07Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon CP-368 Bulk Compound
This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon CP-434R Bulk Compound
Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon R32481R014 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, ..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 51268R020P 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Silicone RubberThickness:Side 1: Skim CoatSide 2: Skim Coat + 0.010" uncuredThis data Represents typical values for the product..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
|
Arlon CP-427R Silicone Rubber
bulk compound
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate..
|
|||
| Dielectric Strength |
15.7
kV/mm @Thickness 3.17 mm |
400
kV/in @Thickness 0.125 in |
|
|
Ineos Nova 5124 High Impact Polystyrene
(discontinued **)
Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C ..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or..
|
|||
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
|
Arlon 55090R028 0.028 (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr..
|
|||
| Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
|
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)&
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data ..
|
|||