Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60112 |
RedEye On Demand PC/ABS for FDM Rapid Prototyping This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the .. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® B 35 FA 000000 Nylon 6, Film Grade PA 6, film , medium viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Applicati.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BC 30 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, rapid processing, higher notched impact strength than B 30 S / B 31 SK in dry and conditioned state, impact-modified |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | Conditioned; IEC 60243-1 |
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6 PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber PA 66, injection molding grade, 15% glass fibers |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | K20/P20; IEC 60243-1 |
Styrolution Luran® S 757 G Q43 White 36609 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
Covestro Apec® 1803 Polycarbonate UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® BG-35 PA6-GF35 Product description: Grilon BG-35 is a heat stabilized PA6 injection molding grade with 35% glass fibers. Grilon BG-35 has the following important properties: High stiffness Good surface finishEasy.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GV 10 HWCP 10% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GV 15 HWCP 15% Glass Fiber Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GVZ 30 HWCP 30% Glass Fiber Z-Qualities Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 GV 40 HWCP 40% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 MR 409 HWCP 40% Mineral Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LV-50H FWA black 9225 PA12-GF50 Product description: Grilamid LV-50H FWA black 9225 is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® LVX-65H SST black 9288 PA12-GF65 Product description: Grilamid LVX-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following .. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 3817 black 9992 PA12 Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe.. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 60243-1 |
Covestro Bayblend® KU 1-1446* Polycarbonate + ABS Developmental productGrade with improved low-temperature impact strength and petrol resistance for automotive partsin version BBS904 suitable for extrusion/extrusion blow molding and electroplating .. |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | IEC 243-1 |
CP-Polymer-Technik Wellamid® 6600 GV 10 HWCP 10% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Dielectric Strength | 35.0 kV/mm | 889 kV/in | dry; IEC 60243-1 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |