Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Asia Pacific) Thermally conductive mineral filled PPS FR compound |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PPS Eco-FR compound |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
PLC 0; UL 746 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.810 mm |
>= 120 sec @Thickness 0.0319 in |
ALL |
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl PX5622 PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. Good flow and surface aesthetics. UL94 V0/5VA/5VB. RTI Elec/Imp/Str 65. Suitable for E/E market indoor/outdoor applications.This da.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East) |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM ATX200R PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend with internal mold release. RoHS compliant. UL94 V0 Listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® 4521 PBT VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® IQNH4560 PBT (Asia Pacific) Valox* IQNH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* iQ PBT resin. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 7500-105 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.70 mm |
>= 120 sec @Thickness 0.0669 in |
UL PLC 0 (120+ sec) |
Sumitomo Bakelite North America RX® 3-2-520F-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX1265 PPE+PS Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics NORYL PX1265 PPE+PS (Asia Pacific) Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | PLC code 0; UL 746A |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.05 mm |
>= 120 sec @Thickness 0.120 in |
UL PLC 0; UL PLC 0 |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific) Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
(BK) |
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol.. |