Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 120 sec Product List

Electrical Properties

Tips: 30 items are displayed at most.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC 0; UL 746
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL V02570 PPE+HIPS
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746
Solvay Specialty Polymers Amodel® AFA-6145 V0 Z Polyphthalamide (PPA), 45% Glass Fiber
Amodel® AFA-6145 V0 Z is a 45% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics ULTEM CRS5111 PEI (Asia Pacific)
10% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5 VA listing.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics ULTEM LTX300B PEI (Asia Pacific)
Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC code 0; UL 746A
SABIC Innovative Plastics Valox® 735 PBT
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics Valox® 830 PBT (Asia Pacific)
30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+PS
LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses).
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC code 0; UL 746A
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA
10% Glass Reinforced PPE+PA Alloy.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL HS2000X PPE+PS
PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific)
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL NH7010 PPE+PS
Noryl* NH7010 resin is a modified PPE-PS blend that exhibits an excellent balance of non-halogenated flame retardance, high heat resistance, good flow, and low specifc gravity for light weight parts..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS
LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses).
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX2926 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_PX2926 compound is a reinforced high modulus PPE+PS. 5VA rated at 2.5 in black and at 3.0 in gray.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC code 0; UL 746A
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific)
Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad..
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
UL 746A
SABIC Innovative Plastics LNP VERTON RV00AXX9 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AXX9 is a compound based on PA 66 resin containing Long Glass Fiber.
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC code 0; UL 746A
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Hot Wire Ignition, HWI >= 120 sec

@Thickness 1.50 mm
>= 120 sec

@Thickness 0.0591 in
(BK)
Hexion Bakelite™ PF 2836 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed &nbs
Phenolic molding compound, inorganically/organically filled, increased heat resistance, increased tracking resistance, low shrinkage and post shrinkage, improved electrical properties, UL listed mol..
Copyright © lookpolymers.com All Rights Reserved