Polymer Property : Insulation Resistance = 100 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Insulation Resistance 100 - 1.00e+12 ohm
100 - 1.00e+12 ohm
Average value: 2.23e+10 ohm Grade Count:70
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Insulation Resistance 100 - 1.00e+9 ohm
100 - 1.00e+9 ohm
Average value: 6.71e+7 ohm Grade Count:30
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Insulation Resistance 100 - 1.00e+11 ohm
100 - 1.00e+11 ohm
Average value: 1.67e+10 ohm Grade Count:6
Overview of materials for Nylon 12, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1105-8048 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Insulation Resistance 100 - 100000 ohm
100 - 100000 ohm
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 19/XCF/20 Polyamide 46, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 6/CF/30 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber
Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & ..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 6-8395 Polyamide 12, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Especially suitable at dynamic stress situations.Electrically conductive, s..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-7050 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-7884 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-8082 Polyacetal-copolymer, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Insulation Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber
Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff ..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1301-0825 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1-7956 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1850-7581-1 PBT, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 80-8072 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Insulation Resistance 100 - 100000 ohm
100 - 100000 ohm
Lehmann & Voss LUVOCOM® TPE-7711/GY Thermoplastic elastomer, with carbon fiber, electrically conducting
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Dynamic stressed parts.Bearings, sleeves, sliding elements, chair rollers, handles.Info..
Insulation Resistance <= 100 ohm
<= 100 ohm
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c..