Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.0 kV/mm @Thickness 1.60 mm |
762 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.787 mm |
762 kV/in @Thickness 0.0310 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
(d AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, .. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
cond.; IEC 60243-1 |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
d.a.m.; IEC 60243-1 |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm |
762 kV/in @Thickness 0.0394 in |
d.a.m.; IEC 60243-1 |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 4012G PBT VALOX 4012G is a 10% glass fiber reinforced PBT injection molding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.60 mm |
762 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.60 mm |
762 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East) VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.50 mm |
762 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.60 mm |
762 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.50 mm |
762 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.60 mm |
762 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.50 mm |
762 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 2.00 mm |
762 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm, Temperature 90.0 °C |
762 kV/in @Thickness 0.0394 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3030G BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 1.00 mm, Temperature 90.0 °C |
762 kV/in @Thickness 0.0394 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a.. |
|||
Dielectric Strength | 30.0 kV/mm @Thickness 0.800 mm |
762 kV/in @Thickness 0.0315 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |