Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | 1.00e+17 ohm @Temperature 23.0 °C |
1.00e+17 ohm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Crastin® HR5315HF BK503 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | insulation resistance |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific) XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Solvay Specialty Polymers Hyflon® PFA 450 Fluoropolymer
(discontinued **) Data provided by the manufacturer.Hyflon® PFA 450 has outstanding physical and chemical properties typical of fluoropolymers.Hyflon® PFA 420 |
|||
Surface Resistance | 1.00e+17 - 1.00e+18 ohm | 1.00e+17 - 1.00e+18 ohm | ASTM D257 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
3M Dyneon™ TF 2025 PTFE Paste Extrusion Powder
(discontinued **) Type I PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 300. Average particle size 500µm. Used for liners.Dyneon offers a family of PTFE fine powder paste extrusion resins. Thes.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Techmer ES HiFill FR® PC FR SFX-GREEN 1.0 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM4025 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM4025 compound is a 40% Glass/Mineral filled high modulus grade. DTUL 255F (124C). UL94 V-0/V-1/5VA rated in black and gray only (see thicknesses). |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 6220F Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics ID-50 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Polyplastics FR-PET® B3015FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose Information provided by PolyPlastics. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | IEC 60093 |
Covestro Bayblend® M850 XF PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Eas.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | ASTM D257 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Surface Resistance | 1.00e+17 - 1.00e+18 ohm | 1.00e+17 - 1.00e+18 ohm | ASTM D257 |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |
|||
Surface Resistance | 1.00e+17 ohm | 1.00e+17 ohm | ASTM D257 |
SABIC Innovative Plastics NORYL FN215Z PPE+HIPS (Asia Pacific) PPE + PS, FR foam molding grade |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics 224 Dacron Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Surface Resistance | >= 1.00e+17 ohm | >= 1.00e+17 ohm | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |