Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES HiFill FR® PC FR SFX-GREEN 1.0

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant , Polycarbonate, UV Stabilized
Manufacturer Techmer ES
Trade Name HiFill FR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill FR® PC FR SFX-GREEN 1.0.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantAppearance: GreenInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0060 cm/cm

@Thickness 3.17 mm
0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Elongation at Break 88 %
88 %
ASTM D638
Flexural Yield Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 0.228 GPa
33.0 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm

@Thickness 3.17 mm
12.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+18 ohm-cm
1.00e+18 ohm-cm
ASTM D257
Surface Resistance 1.00e+17 ohm
1.00e+17 ohm
ASTM D257
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149